FIELD: metallurgy.
SUBSTANCE: method consists of dry ore reduction with usage of impact centrifugal crusher till fineness 60-100% class minus 1.0-4.0 mm, leaching of crushed ore by sulfuric acid of concentration 23-40 g/l at content of solid phase 10-70% during 5-120 min, dehydration, washing, neutralisation and crushing leaching agglomerated cake till fineness 60-95% class minus 0.074 mm, flotation of copper minerals at value pH 8.0-11.0.
EFFECT: flotation effectiveness increase.
7 cl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PROCESSING OF SULPHIDE-OXIDISED COPPER ORES | 2007 |
|
RU2337159C1 |
METHOD OF PROCESSING OF SULPHIDE OXIDISED COPPER ORES | 2007 |
|
RU2337160C1 |
METHOD OF FLOTATION CONCENTRATION OF CAKE OF SULPHURIC ACID LEACHING OF COPPER ORE | 2007 |
|
RU2350396C2 |
METHOD OF PRODUCTION OF CATHODE COPPER OUT OF SULPHIDE OXIDISED COPPER ORES | 2007 |
|
RU2336344C1 |
METHOD OF DIFFERENTIAL FLOTATION OF COPPER MINERALS FROM HARD-CLEANING COPPER ORE | 2007 |
|
RU2352402C2 |
PROCESSING METHOD OF SULPHIDE-OXIDATED COPPER ORES WITH COPPER AND SILVER EXTRACTION | 2009 |
|
RU2439177C2 |
PROCEDURE FOR PROCESSING MIXED COPPER ORE | 2009 |
|
RU2418872C2 |
PROCEDURE FOR EXTACTION OF METALS FROM GOLD CONTAINING SULPHIDE-OXIDISED COPPER ORES | 2009 |
|
RU2428493C1 |
METHOD OF PRODUCTION OF CATHODE COPPER OUT OF SULPIDE OXIDISED COPPER ORES | 2007 |
|
RU2336345C1 |
PROCEDURE FOR PROCESSING ANTIMONY-ARSENIC SULPHIDE GOLD CONTAINING ORE | 2010 |
|
RU2432407C1 |
Authors
Dates
2009-04-20—Published
2007-04-16—Filed