FIELD: construction.
SUBSTANCE: raw mix contains binder, water and additive, additionally contains filler - calcium sulfate dihydrate. Binder used is anhydrous calcium sulfate, and additive is semiaquatic calcium sulfate at the following ratio of components, wt %: calcium sulfate dihydrate 40-56; anhydrous calcium sulfate 24-35; semiaquatic calcium sulfate 1.5-5; water - the rest.
EFFECT: increased strength of material.
1 tbl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
RAW MIXTURE FOR MANUFACTURE OF UNSHRINKABLE CONSTRUCTION MATERIAL | 2007 |
|
RU2384541C2 |
EXPANSION ADDITIVE, HYDRAULIC BINDER WITH INDICATED ADDITIVE, AND A METHOD FOR PREPARATION THEREOF | 2002 |
|
RU2211194C1 |
METHOD OF PRODUCTION OF HIGH-EARLY-STRENGTH PORTLAND CEMENT AND METHOD OF PRODUCTION OF CONCRETE ON BASE OF THIS CEMENT | 2005 |
|
RU2304562C2 |
COMPOSITION FOR THE MANUFACTURE OF WATERPROOF FACING GYPSUM PRODUCTS | 2022 |
|
RU2787245C1 |
COMPLEX ADDITIVE FOR MODIFYING GYPSUM BINDING MATERIALS | 2010 |
|
RU2439016C1 |
DRY MORTAR FOR PREPARATION OF CELLULAR CONCRETE | 2008 |
|
RU2392245C1 |
METHOD OF PREPARATION OF DRY FINE FROTHING AGENT AND METHOD OF PREPARATION OF DRY RAW MIX FOR FOAM CONCRETE WITH USE OF THIS FROTHING AGENT | 2007 |
|
RU2342347C2 |
METHOD OF MANUFACTURE OF CONSTRUCTION STRUCTURES | 1992 |
|
RU2039021C1 |
MIXTURE OF MAKING LIGHT CONCRETE AND LIGHT CONCRETE | 2008 |
|
RU2399598C2 |
ADDITIVE LOWERING SHRINKAGE AND IMPARTING DIMENSIONAL STABILITY TO HARDENING CEMENT-WATER SYSTEMS AND ITS APPLICATION METHOD | 2002 |
|
RU2225375C2 |
Authors
Dates
2009-04-20—Published
2007-09-03—Filed