FIELD: manufacture of construction materials. SUBSTANCE: calcium sulfate, mineral and chemical additives are used. Earthy gypsum is used as calcium sulfate dehydrate in proportion of 0.5-1,5 parts of the whole mass. Glass powder and Portland-cement are used as mineral additives in proportion of 0.5-1.5 each of the whole mass; LST powder as chemical additive in the same proportion as the above additives. Moreover, fine-crystal fraction structure (2-10 mm) gypsum rock (heated up to 160-170 C) is introduced in the amount of 35-45 percent of building plaster. EFFECT: higher durability and lower prime cost.
Title | Year | Author | Number |
---|---|---|---|
RAW MATERIALS MIXTURE FOR MANUFACTURING OF CAST GYPSUM ARTICLES AND METHOD FOR ITS PRODUCTION | 1992 |
|
RU2057736C1 |
ANHYDRIDE CEMENT | 1993 |
|
RU2070170C1 |
BINDER | 0 |
|
SU1451118A1 |
BINDER | 0 |
|
SU730643A1 |
LIQUID-GLASS COMPOSITION | 2014 |
|
RU2568446C1 |
CRUDE MIXTURE FOR PRODUCING NON-AUTOCLAVED AERATED CONCRETE AND METHOD OF PRODUCING NON-AUTOCLAVED AERATED CONCRETE | 2012 |
|
RU2536693C2 |
METHOD OF PRODUCING HYDROPHOBIC CEMENT WITH IMPROVED STRENGTH CHARACTERISTICS | 2009 |
|
RU2419592C1 |
METHOD OF CALCIUM SULFATE PRODUCING | 1991 |
|
RU2023668C1 |
GYPSUM PLATE AND METHOD OF ITS MANUFACTURING | 2014 |
|
RU2617819C2 |
COMPOSITION FOR BUILDING ARTICLE MAKING | 2000 |
|
RU2182567C1 |
Authors
Dates
1995-07-09—Published
1992-04-08—Filed