FIELD: construction.
SUBSTANCE: charge includes the following components, wt %: talc 74.0-76.0; clay 2.0-4.0; carbonic acid barium 6.0-10.0; calcium borate 2.0-4.0; soda 2.0-4.0; borax 6.0-10.0.
EFFECT: reduction of ceramics burning temperature.
1 tbl