FIELD: chemistry.
SUBSTANCE: present invention relates to composition of mixtures for making enamel coating on cast iron and steel objects. The mixture for making enamel coating contains frit, clay and nepheline sludge, with the following ratio of components, wt %: frit- 87.0-89.0; clay - 3.0-4.0; nepheline sludge - 8.0-9.0. Nepheline sludge is characterised by the following composition, wt % SiO2 - 28.0-29.0; Al2O3 - 2.5-3.0; Fe2O3 - 2.5-3.0; CaO - 54.0-55.5; MgO - 1.5-2.5; Na2O - 1.0-1.3; K2O - 0.7-1.0.
EFFECT: increased heat resistance of enamel coating.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
MASS FOR PRODUCTION OF ENAMEL COATING | 2007 |
|
RU2352534C2 |
RAW MIX FOR CERAMSITE PRODUCTION | 2007 |
|
RU2341487C2 |
MIXTURE FOR MAKING ENAMEL COATING | 2008 |
|
RU2384536C1 |
RAW MIXTURE FOR MAKING FACING SLAG-CERAMIC TILES | 2008 |
|
RU2371418C1 |
CERAMIC MIXTURE FOR MAKING FACING TILES | 2010 |
|
RU2417186C1 |
CERAMIC MASS FOR FACING TILE PRODUCTION | 2007 |
|
RU2345034C2 |
CERAMIC MIXTURE | 2006 |
|
RU2329233C1 |
FRIT FOR ENAMEL COVER | 2006 |
|
RU2320579C1 |
RAW MIX FOR EXPANDED CLAY PRODUCTION | 2007 |
|
RU2334708C1 |
CERAMIC MSS FOR FACING TILE PRODUCTION | 2007 |
|
RU2345037C2 |
Authors
Dates
2009-05-27—Published
2007-05-29—Filed