FIELD: chemistry; construction.
SUBSTANCE: invention refers to construction materials as applied to concrete and foam concrete mortars. The process involves phenol waste sulphonation with sulphonating agent represented by 94-96% sulphuric acid in ratio of phenol wastes: sulphonating agent as 1:11/10. The reaction mass is neutralised. Before sulphonation, the phenol waste is treated with d-metal salts at temperature 80-100°C during 0.8-1.0 h. Thereafter organic phase of the prepared reaction mass is separated and sulphonated.
EFFECT: simplified and more efficient process.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING COMPLEX ADDITION FOR CONCRETE MIXTURE | 1996 |
|
RU2132308C1 |
COMPLEX ADDITIVE FOR CONCRETE MIX | 2008 |
|
RU2373165C1 |
METHOD OF PREPARING PLASTICIZER FOR CONCRETE MIXES | 1997 |
|
RU2121465C1 |
METHOD FOR PREPARATION OF CONCRETE MIX PLASTICIZER | 1990 |
|
RU2054401C1 |
GENERATING METHOD OF FLUIDIZING AGENT FOR CONCRETE MIXTURE | 2006 |
|
RU2323907C1 |
COMPLEX ADDITIVE FOR CONCRETE MIXTURE | 1995 |
|
RU2088548C1 |
METHOD OF PRODUCING PLASTICIZER FOR CONCRETE MIXES | 0 |
|
SU1342889A1 |
0 |
|
SU592159A1 | |
METHOD FOR PRODUCTION OF PLASTICIZER | 2003 |
|
RU2245856C1 |
AIR-ENTRAINING ADDITIVE AND METHOD OF OBTAINING THEREOF | 2011 |
|
RU2543231C2 |
Authors
Dates
2009-06-10—Published
2007-12-19—Filed