FIELD: chemistry.
SUBSTANCE: hydrophobic silicon dioxide was obtained pyrogenically, by oxidation in the flame or (which is more preferentially) by hydrolysis in the flame; it contains potassium in the range from 0.000001 to 40 wt %. Silicon dioxide potassium-doped with aerosol hydrophobic can be superficially modified using one or more compounds. The method of such silicon dioxide obtaining and the silicon rubber containing the latter as filler are claimed.
EFFECT: increase of cut-growth resistance and transparency after curing of the liquid rubber mixture.
8 cl, 6 tbl, 6 ex
Title | Year | Author | Number |
---|---|---|---|
SILICON DIOXIDES WITH MODIFIED SURFACE | 2007 |
|
RU2438973C2 |
SILICON DIOXIDES WITH MODIFIED SURFACE | 2007 |
|
RU2445261C2 |
SILOXANES FUNCTIONALIZED WITH AZOCARBONYL | 2015 |
|
RU2688516C2 |
SILICON-CONTAINING AZODICARBOXAMIDES, PRODUCTION AND USE THEREOF | 2016 |
|
RU2727928C2 |
PROCESSING AID FOR THERMOPLASTIC POLYURETHANES | 2009 |
|
RU2520441C2 |
RUBBER MIXTURE | 2012 |
|
RU2612148C2 |
ORGANOSILICON COMPOUNDS, SYNTHESIS AND USE THEREOF | 2006 |
|
RU2417998C2 |
DISPERSION OF HYDROPHOBISATED SILICON DIOXIDE PARTICLES AND GRANULES MADE THEREFROM | 2009 |
|
RU2472823C2 |
METHOD FOR PRODUCING SILICONE-CONTAINING AZODICARBAMIDES | 2011 |
|
RU2559876C2 |
MODIFIED ELASTOMERIC POLYMERS | 2009 |
|
RU2504555C2 |
Authors
Dates
2009-06-20—Published
2005-10-29—Filed