FIELD: mining.
SUBSTANCE: coal is mixed with water and sintering additive in disperser, whereupon it is dehydrated. As coal there are used coal slimes which are enriched by the method of oil agglomeration to ash content 4.0-7.6% wt and sulphur content 0.2-0.3% wt by means of a sintering additive at rate of mixing 1000-1500 rev/min. Produced coal-oil concentrates of dimension 2-3 mm are separated on a sieve, mixed with other grades of enriched coal-oil concentrates and are subject to coking.
EFFECT: upgraded quality of source coal charge, reduced contents of ash and sulphur in source charge and increased strength of coke.
3 cl, 2 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCTION OF THE WATER-METHOD FUEL AND ITS COMPOSITION | 2005 |
|
RU2277120C1 |
METHOD OF SLURRY COAL AND COAL CONCENTRATION | 2012 |
|
RU2494817C1 |
METHOD FOR PREPARATION OF CHARGE FOR COKING | 2020 |
|
RU2735742C1 |
METHOD FOR PREPARING A CHARGE FOR COKING | 2017 |
|
RU2663145C1 |
COKE DUST BRIQUETTING METHOD | 2011 |
|
RU2468071C1 |
BLEND FOR THE PRODUCTION OF METALLURGICAL COKE | 2022 |
|
RU2792812C1 |
METHOD OF PREPARING COAL CHARGE FOR COKING | 2010 |
|
RU2445342C1 |
ADDITIVE TO COKING CHARGE | 2009 |
|
RU2418837C1 |
METHOD FOR CHARGE FORMING FOR FURNACE COKE OBTAINING | 2011 |
|
RU2461602C1 |
0 |
|
SU289117A1 |
Authors
Dates
2009-07-10—Published
2008-04-07—Filed