FIELD: metallurgy.
SUBSTANCE: invention relates to metallurgy, in particular to obtaining boron alloying alloys for alloying of steel, cast iron, etc. A reaction mixture containing 1-40 wt % of a boron-containing component is prepared: one or several borides of one or several elements selected from a group including calcium, magnesium, aluminium, silicon and 60-99 wt % of the metal component, one or several elements selected from a group including calcium, aluminium, titanium, silicon, vanadium, niobium, zirconium, molybdenum, chromium, manganese, cobalt, iron and/or their alloys. Powders are used with the particles of 3 mm maximum. This is followed by a start of an exothermal reaction of burning in the inert atmosphere.
EFFECT: increased yield output and reduction in the content of the detrimental impurities in the alloy.
9 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
ALLOY FOR STEEL MICROALLOYING BY BORON | 2008 |
|
RU2375486C1 |
METHOD FOR OBTAINING TITANIUM-CONTAINING ALLOY FOR STEEL ALLOYING | 2012 |
|
RU2497970C1 |
ALLOY FOR ALLOYING OF STEEL WITH TITANIUM | 2012 |
|
RU2482210C1 |
NITROGEN CONTAINING ALLOY FOR STEEL ALLOYING AND PROCEDURE FOR ITS PRODUCTION | 2008 |
|
RU2395611C2 |
METHOD FOR PRODUCING A COMPOSITE ALLOY BASED ON CHROMIUM NITRIDES | 2022 |
|
RU2798491C1 |
METHOD OF PRODUCING NITROGEN-BEARING ALLOY | 2015 |
|
RU2583980C2 |
METHOD FOR PRODUCTION OF COMPOSITIONAL BORON-CONTAINING ALLOYS FOR STEEL ALLOYING | 0 |
|
SU1770434A1 |
METHOD TO OBTAIN NITROGEN-CONTAINING LIGATURE | 2011 |
|
RU2462526C1 |
PROCESS OF PRODUCTION OF ALLOYING MATERIAL BASED ON SILICON NITRIDE | 2002 |
|
RU2210615C1 |
ALLOY FOR STEEL MICRO-ALLOYING | 2010 |
|
RU2434964C1 |
Authors
Dates
2009-08-27—Published
2007-07-09—Filed