FIELD: mining.
SUBSTANCE: method is in blending of at least 92% ground and 8% of cement by mass and implemented in following succession: in preliminary blending at least 3/5 parts of strengthened ground with water in amount 40-50% from total amount of water and with cement in amount 20-50% from total amount of cement; aging of mixture on air during 20-60 min.; blending of this mixture with mixture of rest components. Strengthened ground mass at first is divided for two parts in ratio "golden section" 0.67 and 0.33; then each part is separately blended with 50% of accepted cement mass, and received two mixtures by means of blending are united into common mass; after that received mixture is blended with specified amount of water, after what finished mixture is aged on air during 20-60 minute before piling and compaction of it into basis of road pavement.
EFFECT: development and creation of method of uniformity increasing by durability of soil cement.
6 dwg
Title | Year | Author | Number |
---|---|---|---|
ROAD POLYMER-CEMENT-SOIL MIX | 2008 |
|
RU2373321C1 |
METHOD OF CONSTRUCTION OF COVERINGS AND BASES OF ROADWAYS AND RUNWAYS | 0 |
|
SU1636497A1 |
METHOD FOR CONSOLIDATING SOIL FOR PAVING | 0 |
|
SU1664972A1 |
METHOD OF CONSTRUCTING THE BEDS AND PAVING OF HIGHWAYS AND AIRFIELDS | 0 |
|
SU804750A1 |
METHOD OF CONSTRUCTING PAVINGS | 0 |
|
SU1458463A1 |
METHOD OF CONSOLIDATING SOIL | 0 |
|
SU1362780A1 |
METHOD OF PAVEMENT BUILDING | 2002 |
|
RU2226584C1 |
METHOD OF PAVEMENT CONSTRUCTION | 0 |
|
SU1664948A1 |
METHOD OF CONSOLIDATING SOIL FOR ROAD BED | 0 |
|
SU1738915A1 |
METHOD FOR CONSTRUCTION OF ROAD SURFACE | 0 |
|
SU1731889A1 |
Authors
Dates
2009-10-27—Published
2008-04-29—Filed