FIELD: chemistry.
SUBSTANCE: bottles are crushed to particle size ranging from 0.001 to 5 mm, mixed with calcium chloride in mass ratio bottle : CaCl2 equal to 20:1.
EFFECT: obtaining new material.
1 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
MIXED ANTI-ICING MATERIAL | 2011 |
|
RU2464293C1 |
METHOD OF PRODUCTION OF THE ANTI-ICING REACTANT | 2005 |
|
RU2277113C1 |
METHOD FOR PRODUCING SOLID DEICING MATERIAL BASED ON TABLE SALT AND CALCINED CALCIUM CHLORIDE (VERSIONS) | 2015 |
|
RU2604033C2 |
METHOD FOR PRODUCING SOLID DEICING MATERIAL BASED ON TABLE SALT AND CALCINED CALCIUM CHLORIDE (VERSIONS) | 2015 |
|
RU2603156C2 |
SORBENT FOR REMOVING RADIONUCLIDES FROM WATER | 2011 |
|
RU2499309C2 |
ANTI-GLAZE COMPOSITION (VERSIONS) AND METHOD OF ITS MANUFACTURING | 2012 |
|
RU2523470C2 |
METHOD FOR PRODUCING SOLID DEICING MATERIAL BASED ON TABLE SALT AND CALCINED CALCIUM CHLORIDE (VERSIONS) | 2015 |
|
RU2604214C2 |
ENVIRONMENTALLY SAFE SNOW REMOVAL COMPOSITION CONTAINING A POROUS STRUCTURE MADE FROM STARFISH | 2018 |
|
RU2698684C1 |
METHOD FOR PRODUCING SOLID DEICING MATERIAL BASED ON TABLE SALT AND CALCINED CALCIUM CHLORIDE (VERSIONS) | 2015 |
|
RU2597100C1 |
METHOD FOR PRODUCING SOLID DEICING MATERIAL BASED ON TABLE SALT AND CALCINED CALCIUM CHLORIDE (VERSIONS) | 2015 |
|
RU2604213C2 |
Authors
Dates
2010-01-10—Published
2007-05-03—Filed