FIELD: construction.
SUBSTANCE: ceramic mass contains loess-like loam, kaolinite clay, phosphorite, at the following ratio of components, wt %: loess-like loam - 88.0-90.0; kaolinite clay - 7.0-8.0; phosphorite - 3.0-4.0.
EFFECT: product strength improvement.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
CERAMIC MIXTURE FOR MAKING FACING TILES | 2010 |
|
RU2418761C1 |
CERAMIC MIXTURE | 2006 |
|
RU2326853C1 |
CERAMIC MIXTURE | 2010 |
|
RU2418762C1 |
CERAMIC MIXTURE | 2010 |
|
RU2420480C1 |
CERAMIC MASS | 2010 |
|
RU2427553C1 |
CERAMIC MIXTURE FOR MAKING FACING TILES | 2009 |
|
RU2388724C1 |
CERAMIC MASS FOR PRODUCTION OF FACING TILES | 2008 |
|
RU2377222C1 |
CERAMIC PASTE FOR MANUFACTURING FINISH TILE | 2008 |
|
RU2375328C1 |
CERAMIC MASS | 2010 |
|
RU2427552C1 |
CERAMIC MIXTURE FOR MAKING FACING TILES | 2010 |
|
RU2424203C1 |
Authors
Dates
2010-04-27—Published
2009-04-16—Filed