FIELD: chemistry.
SUBSTANCE: invention relates to a method of hardening organoboron polymers used in the industry of heat-resistant composite materials. Described is a method of hardening polymethylene-p-triphenyl ether of boric acid at 185-195°C for 2-2.5 hours with a sulphur curing system, with the following composition of components, pts. wt: sulphur - 26.9 - 28.6; thiuram - 11.6-12.3; zinc oxide - 3.9-4.2 and captax - 2.0-2.3 per 100 pts. wt polymethylene-p-triphenyl ether of boric acid.
EFFECT: proposed method avoids release of gas and gaseous products of hardening and therefore improves physical and mechanical properties of the friction product.
1 cl, 6 ex
Title | Year | Author | Number |
---|---|---|---|
POLYMER FRICTION COMPOSITION | 2010 |
|
RU2442802C2 |
EPOXY BINDING AGENT FOR FIBERGLASS | 2007 |
|
RU2339662C1 |
ORGANIC CONCRETE BLEND | 2001 |
|
RU2185346C1 |
HEAT-RESISTANT ANTICORROSION COMPOSITION | 2011 |
|
RU2468053C1 |
POLYMER-CONCRETE MIXTURE | 2004 |
|
RU2266876C1 |
POLYMERIC COMPOSITION FOR FILM COATING | 1990 |
|
RU2022979C1 |
OIL-AND-PETROL-RESISTANT AND COLD-RESISTANT RUBBER MIXTURE | 2018 |
|
RU2688741C1 |
POLYMER-CONCRETE MIXTURE | 1997 |
|
RU2120425C1 |
RUBBER MIX FOR PRODUCTION OF WATERPROOF MATERIALS (VERSIONS) | 2004 |
|
RU2277108C1 |
BUTYL RUBBER-BASED ELASTOMER MATERIAL FOR GAS MASK HOUSING | 2012 |
|
RU2495062C1 |
Authors
Dates
2010-04-27—Published
2007-06-29—Filed