FIELD: construction.
SUBSTANCE: dry construction mix contains the following components, wt %: gypsum binder - construction gypsum 73.0-85.0, slaked lime 10.0-16.0, polycarboxylate, at least one, selected from the following group: sodium polycarboxylate, polycarboxylate Melflux 1641F, GP-1, Sika ViskoCrete 225P and BPS BV T/C 1.3-3.0, carboxymethylcellulose 3.0-5.6, aluminium sulfate 0.4-0.9, sodium gluconate 0.3-1.5, besides it is prepared by mixing specified components in disintegration mixer for 2-3 minutes at speed of mixer rotation of 2500-3000 rpm. Method for application of specified mix is characterised by the fact that it is added to light porous filler with fraction of at least 5 mm at the ratio of weight of specified filler to dry construction mix in the range of 1.8-6.4, at the same time filler is previously wetted with water taken to produce water and gypsum ratio in the range of 0.32-0.59.
EFFECT: reduced power inputs in process of drying, low consumption of binding material, increased strength, water resistance and thermal resistance of produced heat insulation material.
4 cl, 3 tbl, 14 ex
Authors
Dates
2010-11-20—Published
2009-05-13—Filed