FIELD: chemistry.
SUBSTANCE: polymeric mixed composition is obtained through co-extrusion of polyamide in a melt with a modifying additive. The modifying additive is a mixture of polyethylene with a copolymer of ethylene with C3-8 olefin in ratio of components (pts. wt) between 1:9 and 9:1. Before co-extrusion in a melt with polyamide 6, the modifying additive undergoes reaction extrusion. 0.3-3 wt % polar monomer and 0.1-0.6 wt % organic peroxide are further added to the composition at the co-extrusion step at reaction extrusion temperature of 170-240°C and the following ratio of components in the polyamide composition, wt %: polyamide 6 - up to 100, modifying additive 15-45. Co-extrusion temperature 235-275°C.
EFFECT: invention reduces melt flow index of the molten mass, enables to obtain impact resistant and petroleum product-resistant polyamide materials and also simplifies technology of producing said materials.
4 cl, 2 tbl, 24 ex
Title | Year | Author | Number |
---|---|---|---|
POLYAMIDE COMPOSITION | 2009 |
|
RU2409604C2 |
METHOD OF PREPARING REINFORCED POLYAMIDE COMPOSITION | 1999 |
|
RU2152411C1 |
METHOD FOR PRODUCTION OF PLASTIC TANKS FOR PETROLEUM PRODUCTS | 2004 |
|
RU2278787C2 |
METAL PIPE, USE THEREOF, POLYAMIDE MIXTURES AND ARTICLE MOULDED THEREFROM | 2015 |
|
RU2685208C2 |
POLYESTER COMPOSITE MATERIAL | 2008 |
|
RU2408629C2 |
METHOD FOR PRODUCING GLASS-FILLED POLYAMIDE COMPOSITION AND GLASS-FILLED POLYAMIDE COMPOSITION | 2015 |
|
RU2618255C1 |
APPLICATION OF COMPOSITION FOR CONTACT WITH SUPERCRITICAL MEDIA | 2009 |
|
RU2543205C2 |
THERMOPLASTIC COMPOSITION | 1997 |
|
RU2129134C1 |
PIPELINE | 2007 |
|
RU2469236C2 |
GLUES, OBTAINED FROM POLYMER SYSTEMS | 2010 |
|
RU2557232C2 |
Authors
Dates
2011-01-10—Published
2009-01-19—Filed