FIELD: metallurgy.
SUBSTANCE: procedure for production of multi-layer coating for cutting tool consists in vacuum-plasma application of three-layer coating. As a lower layer nitride of titanium and iron is applied at pressure of nitrogen in a chamber of the installation 7.5·10-4 Pa and temperature 600°C. Same nitride alloyed with aluminium is applied as an intermediate layer at pressure of nitrogen of 7.5·10-4 Pa and temperature 550°C in the chamber of the installation. As an upper layer nitride of titanium and aluminium is applied at pressure of nitrogen in a chamber of the installation 4.3·10-3 Pa and temperature 500°C.
EFFECT: increased functionality of tool and upgraded quality of treatment.
2 cl, 1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
PROCEDURE FOR PRODUCTION OF MULTI-LAYER COATING FOR CUTTING TOOL | 2010 |
|
RU2428509C1 |
METHOD OF PRODUCING MULTI-LAYER COAT FOR CUTTING TOOL | 2009 |
|
RU2410465C1 |
PROCEDURE FOR PRODUCTION OF MULTI-LAYER COATING FOR CUTTING TOOL | 2010 |
|
RU2424359C1 |
PROCEDURE FOR CUTTING TOOL MULTI-LAYER COATING | 2009 |
|
RU2414527C1 |
PROCEDURE FOR CUTTING TOOL MULTI-LAYER COATING | 2009 |
|
RU2414532C1 |
PROCEDURE FOR CUTTING TOOL MULTI-LAYER COATING | 2009 |
|
RU2414530C1 |
PROCEDURE FOR PRODUCTION OF MULTI-LAYER COATING FOR CUTTING TOOL | 2010 |
|
RU2424365C1 |
PROCEDURE FOR PRODUCTION OF MULTI-LAYER COATING FOR CUTTING TOOL | 2010 |
|
RU2430988C1 |
PROCEDURE FOR PRODUCTION OF MULTI-LAYER COATING FOR CUTTING TOOL | 2010 |
|
RU2428507C1 |
PROCEDURE FOR PRODUCTION OF MULTI-LAYER COATING FOR CUTTING TOOL | 2010 |
|
RU2424363C1 |
Authors
Dates
2011-07-20—Published
2010-04-13—Filed