FIELD: construction.
SUBSTANCE: mass for enamel coating production includes the following components, wt %: frit 90.17-92.63; nickel oxide 0.3-0.8; bentonite 2.5-3.5; borax 0.03-0.07; bone ash 4.0-6.0. Heat resistance makes 8-10 thermal cycles when heated up to 450°C and cooled on air.
EFFECT: improved heat resistance of enamel coating.
2 tbl