FIELD: metallurgy.
SUBSTANCE: procedure consists in fluoridation of raw material by sintering with fluoride agent. Upon fluoridation product is crumbled, dissolved in distilled water and filtered. Produced solution is settled with ammonia at pH 8÷9, sediment is mixed with chloride of ammonia and baked at 220-270°C during 5 hours.
EFFECT: production of titanium oxide of rutile form and iron oxide.
3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PROCESSING OF RAW MATERIALS CONTAINING TITANIUM | 2008 |
|
RU2365647C1 |
METHOD TO PROCESS TITANIUM-SILICON-CONTAINING STOCK | 2008 |
|
RU2377332C2 |
METHOD FOR OBTAINING TITANIUM DIOXIDE FROM ILMENITE | 2021 |
|
RU2770576C1 |
METHOD OF PREPARING TITANIUM-CONTAINING STOCK | 1998 |
|
RU2139249C1 |
METHOD OF PROCESSING TITANIUM-CONTAINING MINERAL RAW MATERIALS | 2016 |
|
RU2623974C1 |
METHOD OF PROCESSING TITANIUM-CONTAINING MINERAL RAW MATERIALS | 2019 |
|
RU2717418C1 |
METHOD OF COMPLEX PROCESSING OF TITANIUM-CONTAINING MINERAL RAW MATERIALS | 2016 |
|
RU2620440C1 |
METHOD OF PROCESSING TITANIUM-CONTAINING MINERAL STOCK | 1998 |
|
RU2136771C1 |
METHOD OF PREPARING IRON AND TITANIUM | 1998 |
|
RU2144504C1 |
METHOD FOR BIFLUORIDE TREATMENT OF RARE AND RARE-EARTH MINERAL MATERIAL | 2014 |
|
RU2576710C1 |
Authors
Dates
2011-10-27—Published
2010-12-03—Filed