FIELD: machine building.
SUBSTANCE: proposed method consists in securing strip on vane leading edges, all along their length, said strip being made up of separate shaped stellite plates cut from solid shaped casting and butted together. One-piece stellite casting is divided into two or more sections. Said plates cut from one ingot section are arranged sequentially from vane apex starting from plates from mould closest to periphery. Plate face closest to mould periphery is arranged on vane apex side.
EFFECT: higher reliability due to longer life of anti-erosion protection.
2 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF STRENGTHENING SURFACE OF UPPER PART OF TURBINE BLADE AIRFOIL PORTION | 2003 |
|
RU2241123C1 |
METHOD OF STRENGTHENING SURFACE OF UPPER PART OF TURBINE BLADE FEATHER | 2005 |
|
RU2297538C2 |
PROTECTION OF STEAM TURBINE BLADES AGAINST STEAM DROP EROSION | 2013 |
|
RU2545878C2 |
PROCESS OF TREATMENT OF PARTS | 1997 |
|
RU2115763C1 |
BLADES OF WET-STEAM TURBINE STAGE | 0 |
|
SU1507991A1 |
METHOD OF STRENGTHENING SURFACE OF INLET EDGES OF TURBINE BLADES | 1990 |
|
RU2030599C1 |
BLADE OF WET STEAM TURBINE | 0 |
|
SU1219830A1 |
AMORPHOUS ALLOY ON COBALT BASIS | 2014 |
|
RU2631563C2 |
METHOD TO RECONDITION STEAM TURBINE VANES FROM ALLOYED STEELS | 2009 |
|
RU2426631C1 |
METHOD FOR RESTORING STEAM TURBINE BLADES | 2003 |
|
RU2251476C1 |
Authors
Dates
2011-11-10—Published
2010-03-17—Filed