FIELD: chemistry.
SUBSTANCE: method involves cathodic electrodeposition from a water-base lacquer composition containing 60-70% solution in a mixture of ethylglycoacetate and butanol epoxyamino-rubber adduct modified with malamine-formaldehyde resin K-421-02, an organic acid and distilled water, and hardening the coating. The lacquer composition additionally contains 75-85% solution in toluene bis(dicresoxy-phosphine-oxy)dibutoxy titanium, with the following ratio of components in wt %: 60-70% solution in a mixture of ethylglycol acetate and butanol epoxyamino-rubber adduct, modified with melamine-formaldehyde resin K-421-02 - 1.6-11.0; 75-85% solution in toluene bis(dicresoxy-phosphine-oxy)dibutoxy titanium 0.008-1.1; organic acid 0.008-1.1; distilled water - the rest. Electrodeposition is carried out at voltage 60-200 V for 3-60 s.
EFFECT: designing a method of obtaining coatings mainly on arrow-shaped bullets, having high corrosion resistance in NaCl solution and enabling complete sealing of cartridges with anaerobic sealants.
3 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
WATER-DILUABLE COMPOSITION | 2013 |
|
RU2567290C2 |
MODIFYING ADDITIVE FOR WATER-BASED POLYORGANOSILOXANE POLYMER AND COPOLYMER OF BUTADIENE WITH STYRENE | 2008 |
|
RU2391368C1 |
WATER-DISSOLUBLE COMPOSITION FOR ELECTRODEPOSITION-MEDIATED FORMATION OF COATINGS | 2002 |
|
RU2226204C1 |
WATER-DILUTING COMPOSITION FOR PREPARING COVER BY ELECTROLYTIC PRECIPITATION METHOD | 2004 |
|
RU2279457C1 |
WATER DILUTED COMPOSITION FOR ANTIFRICTION COATINGS | 1990 |
|
RU2083615C1 |
ANTICORROSION PROTECTIVE POLYMER COATING AND METHOD OF ITS APPLICATION ONTO SURFACE OF STEEL CASE OF SMALL ARMS CARTRIDGES | 2010 |
|
RU2439114C1 |
0 |
|
SU1781265A1 | |
METHOD OF DEPOSITING POLYMER COATS | 0 |
|
SU1684355A1 |
WATER DILUTABLE PAINT AND VARNISH COMPOSITION FOR COATING | 1993 |
|
RU2031916C1 |
COMPOSITION FOR SEALING ARTICLES OF ALUMINUM AND COPPER ALLOYS | 2004 |
|
RU2276176C1 |
Authors
Dates
2012-01-27—Published
2010-05-25—Filed