FIELD: oil and gas industry.
SUBSTANCE: in manufacturing method of siliceous proppant, which involves charge grinding, granulation and baking of granules, natural highly siliceous sand or its mixture with quartzite in quantity of 1-25% of mass of mixture at SiO2 content in the charge of not less than 87 wt % is used as charge; grinding is performed to the size of not more than 10 mcm at fraction content of not more than 5 mcm, which is not less than 50 wt %, and calcination - at 1120-1300°C at heating rate of 1000-2500°C/h and cooling rate of 1000-2000°C/h. Siliceous proppant is characterised by the fact that it has been obtained by means of the above method; at that, content of christobalite in calcined granules does not exceed 10 vol %.
EFFECT: decreasing proppant density at maintaining allowable strength values of granules.
3 cl, 2 ex, 1 tbl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
ULTRALIGHT SILICEOUS MAGNESIUM-CONTAINING PROPPANT MANUFACTURING METHOD | 2013 |
|
RU2535540C1 |
MANUFACTURING METHOD OF LIGHT-WEIGHT SILICEOUS PROPPANT, AND PROPPANT | 2010 |
|
RU2446200C1 |
FEED FOR MANUFACTURING OF LIGHT-PROOF SILICON PROPPANT AND PROPPANT | 2017 |
|
RU2650149C1 |
LIGHT SILICEOUS MAGNESIUM-CONTAINING PROPPANT MANUFACTURING METHOD | 2014 |
|
RU2547033C1 |
MANUFACTURING METHOD OF LIGHT-WEIGHT SILICEOUS PROPPANT AND PROPPANT | 2016 |
|
RU2623751C1 |
FEED FOR MANUFACTURING OF LIGHT-PROOF SILICON PROPPANT AND PROPPANT | 2016 |
|
RU2653200C1 |
RAW BATCH FOR MAGNESIAN-QUARTZ PROPPANT PRODUCTION | 2017 |
|
RU2646910C1 |
METHOD FOR MANUFACTURING OF LIGHT-WEIGHT HIGH-SILICA MAGNESIUM-CONTAINING PROPPANT FOR PRODUCTION OF SHALE HYDROCARBONS | 2012 |
|
RU2513792C1 |
CHARGE FOR THE MANUFACTURE OF CERAMIC PROPPANT AND PROPPANT | 2022 |
|
RU2781688C1 |
METHOD OF PRODUCING CERAMIC PROPPANTS | 2013 |
|
RU2515661C1 |
Authors
Dates
2012-03-20—Published
2010-08-10—Filed