FIELD: textile, paper.
SUBSTANCE: method to produce modified cellulose for use in products from paper or paper web includes extraction of wood chips with a fluid containing water, at the temperature of 20° - 120°C from 5 minutes to 10 hours, to reduce content and remove hemicellulose to get processed wood chips. Then sulfate boiling is carried out, and the processed wood chips are bleached to produce a modified sulfate cellulose. Besides, the amount of hemicellulose contained in the modified bleached sulfate cellulose makes from 4% to 9% of the weight of the dry modified sulfate cellulose.
EFFECT: method improvement.
10 cl, 4 tbl, 4 ex, 2 dwg