FIELD: metallurgy.
SUBSTANCE: electrolyte contains, g/L: chromic anhydride 30-35, boric acid 1-2, 11-trimethyl-4-oxyfluoranten-3-sulfonic acid 0.7-2.0, O,O-diethyl-S-benzyl thiophosphate 1.5-3.6.
EFFECT: increased anticorrosion properties of protective ematal coatings.
1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| ALUMINUM AND ITS ALLOYS EMATALIRISING ELECTROLYTE | 2005 |
|
RU2297475C1 |
| ELECTROLYTE FOR SIMULTANEOUS DEGREASING AND ETCHING ALUMINIUM AND ALLOYS THEREOF BEFORE ANODIC TREATMENT | 2008 |
|
RU2395627C1 |
| ELECTROLYTE FOR EMATALIZING ALUMINIUM AND ITS ALLOYS | 0 |
|
SU1133313A1 |
| METHOD FOR ENAMELLING ALUMINIUM ALLOY ARTICLES | 1990 |
|
RU2024652C1 |
| ELECTROLYTE OF ALUMINIUM AND ITS ALLOYS ANODIC TREATMENT | 2009 |
|
RU2416680C1 |
| ZINK PLATING ELECTROLYTE SOLUTION | 0 |
|
SU905335A1 |
| ELECTROLYTE FOR BLACK CHROMATIZING OF ZINC | 1997 |
|
RU2137861C1 |
| METHOD OF ENAMELLING ALUMINIUM ALLOY ARTICLES | 0 |
|
SU1120034A1 |
| ELECTROLYTE FOR ANODE-PLATING OF ALUMINIUM ALLOYS | 0 |
|
SU617493A1 |
| ELECTROLYTE FOR ANODIZING ALUMINUM AND ITS ALLOYS | 2005 |
|
RU2287027C1 |
Authors
Dates
2012-07-20—Published
2011-01-13—Filed