FIELD: electrochemical treatment of aluminium alloys. SUBSTANCE: electrolyte bath contains, g/l: boric acid, 1-2; chromic acid, 15-20; sulfurous cobalt, 0.1-1.0; water, the balance. Voltage 55 V, temperature 40-55 C, duration, 40-50 min. EFFECT: higher efficiency. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
ALUMINUM AND ITS ALLOYS EMATALIRISING ELECTROLYTE | 2005 |
|
RU2297475C1 |
ELECTROLYTE FOR EMATAL COATING OF ALUMINIUM AND ITS ALLOYS | 2011 |
|
RU2456384C1 |
ELECTROLYTE FOR EMATALIZING ALUMINIUM AND ITS ALLOYS | 0 |
|
SU1133313A1 |
METHOD OF COMPACTION AND COLORATION OF ANODIZED PRODUCTS FROM ALUMINIUM OR ITS ALLOYS | 0 |
|
SU1819917A1 |
METHOD OF ENAMELLING ALUMINIUM ALLOY ARTICLES | 0 |
|
SU1120034A1 |
METHOD OF APPLYING ELECTROCONDUCTIVE PROTECTIVE COATING ON ALUMINIUM ALLOYS | 2023 |
|
RU2817277C1 |
METHOD OF FIRMING ANODE-OXIDE COATING OF ITEM OUT OF ALUMINIUM AND ITS ALLOYS | 2009 |
|
RU2383663C1 |
SOLUTION FOR TIGHTENING OF ANODE-OXIDE FILM ON ALUMINIUM AND ITS ALLOYS | 1993 |
|
RU2061801C1 |
PROCEDURE FOR HARD ANODISING ITEMS OUT OF ALUMINIUM ALLOYS | 2008 |
|
RU2390588C1 |
ELECTROLYTE FOR SIMULTANEOUS DEGREASING AND ETCHING ALUMINIUM AND ALLOYS THEREOF BEFORE ANODIC TREATMENT | 2008 |
|
RU2395627C1 |
Authors
Dates
1994-12-15—Published
1990-12-21—Filed