FIELD: metallurgy.
SUBSTANCE: steel contains carbon, silica, manganese, sulphur, phosphorus, chrome, nickel, copper, molybdenum, titanium, aluminium, calcium, boron and iron at the following component ratio, wt %: carbon 0.33 -0.45, manganese 0.90 - 1.30, silica 0.15 - 0.37, phosphorus not more than 0.030, sulphur from more than 0.01 to 0.040, chrome 0.15 - 0.25, nickel not more than 0.30, copper not more than 0.30, molybdenum 0.02 - 0.04, titanium 0.01 - 0.045, aluminium 0.02 - 0.05, boron 0.0010 - 0.0030, calcium 0.0001 - 0.005, ferrum the rest. For steel components the following ratio is satisfied [S] / [Al]+[Ti]+[Ca] = 0.3 - 0.5.
EFFECT: increase of rolled products application properties and yield ratio at steel casting, provision of specified degree of hardness penetration.
1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING BORON-CONTAINING STEEL | 2011 |
|
RU2492248C2 |
BORON STEEL MAKING METHOD | 2011 |
|
RU2477324C1 |
LOW-ALLOY BORON STEEL OF HIGH TREATABILITY | 2008 |
|
RU2363753C1 |
CORROSION RESISTANT STEEL FOR OIL-GAS EXTRACTING EQUIPMENT | 2010 |
|
RU2437954C1 |
ROUND ROLLED STOCK FROM BORON-CONTAINING STEEL OF INCREASED HARDENING CAPACITY | 2011 |
|
RU2469106C1 |
METHOD FOR PRODUCING ROUND ROLLED STOCK OF BORON-CONTAINING STEEL WITH INCREASED DUCTILITY | 2017 |
|
RU2636542C1 |
HOT-ROLLED COIL STOCK PRODUCTION METHOD | 2019 |
|
RU2727398C1 |
STEEL | 2009 |
|
RU2425169C2 |
TUBE STOCK OUT OF ALLOYED BORON CONTAINING STEEL | 2006 |
|
RU2337151C1 |
HOT-ROLLED SHEET PRODUCTION METHOD | 2023 |
|
RU2813917C1 |
Authors
Dates
2012-08-10—Published
2010-12-03—Filed