FIELD: metallurgy.
SUBSTANCE: mixture contains the following components, wt %: magnesium 12-17, graphite 15-20, boric anhydride 12-15, calcium hydride 7-11, boron nitride 10-20, ferrophosphorus 8-12, and ferrosilicium is the rest.
EFFECT: invention allows improving stability of modifying effect, wear resistance and friction properties of cast-iron.
2 tbl