FIELD: process engineering.
SUBSTANCE: proposed method comprises subjecting natural leather to low-temperature plasma of high-frequency induction discharge for 30-120 seconds at discharge chamber pressure of 40-60 Pa at flow rate of plasma-forming argon of 0.04-0.08 g/s at current of 0.3-0.9 A. Then, it is subjected to low-temperature plasma of high-frequency induction discharge for 60-600 seconds at discharge chamber pressure of 13.3-26.6 Pa at flow rate of plasma-forming argon of 0.02-0.06 g/s at current of 0.3-0.7 A and voltage of 1.3-3.0 kV.
EFFECT: ruled out grain breaks.
2 dwg, 1 tbl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR DRESSING OF LEATHER SEMI-FINISHED GOODS | 2008 |
|
RU2399679C2 |
METHOD OF NATURAL LEATHER SHOE UPPER PROCESSING AFTER STRETCHING AND LASTING OPERATIONS | 2006 |
|
RU2356482C2 |
METHOD OF PRODUCING TEXTILE MATERIAL WITH ANTIBACTERIAL PROPERTIES FOR OVERALLS | 2016 |
|
RU2619704C1 |
METHOD TO MANUFACTURE NATURAL LEATHER | 2008 |
|
RU2378386C2 |
LEATHER FINISHING PROCESS | 2005 |
|
RU2298040C1 |
METHOD OF METAL CORD TREATMENT | 2007 |
|
RU2366759C2 |
METHOD TO STRENGTHEN POLYPROPYLENE THREAD | 2010 |
|
RU2421556C1 |
METHOD FOR PRODUCTION OF KNITTED MATERIAL WITH ANTIBACTERIAL PROPERTIES | 2019 |
|
RU2703631C1 |
METHOD OF WOOL TREATMENT | 2008 |
|
RU2378422C2 |
SKIN TREATMENT PROCESS | 1997 |
|
RU2127763C1 |
Authors
Dates
2012-09-10—Published
2011-02-21—Filed