FIELD: chemistry.
SUBSTANCE: mass for obtaining enamel coating contains the following components, wt %: frit 66.0-67.0; mullite 14.0-16.0; quartz sand - 14.0-16.0; tin dioxide - 3.0-4.0.
EFFECT: increase of enamel thermal resistance.
1 tbl