FIELD: construction.
SUBSTANCE: ceramic mass includes plastic clay, kaolin, swollen ground perlite, phosphogypsum and glycerine, at the following ratio of components, wt %: plastic clay 66.5-67.2; kaolin 4.0-4.4; swollen ground perlite 24.0-26.0; phosphogypsum 3.0-4.0, glycerine 0.4-0.5.
EFFECT: lowering of products burn temperature.
1 tbl