FIELD: chemistry.
SUBSTANCE: invention relates to production of concrete aggregates. In the method of producing coarse aggregate for concrete, involving depositing a layer of a mineral binder-based mixture onto the surface of an aggregate, followed by hardening thereof, the aggregate used is blast-furnace slag chips and the mineral binder-based mixture is a portland cement-slag and sand mixture, which is obtained by grinding blast-furnace slag, taken in weight ratio of 1:3-1:2, with water-to-cement ratio of 0.8-1.2.
EFFECT: high adhesion of the aggregate to hardened cement paste of the concrete.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MANUFACTURING DECORATIVE FILLER | 2007 |
|
RU2334711C1 |
METHOD OF PRODUCTION OF LARGE-SIZE FILLER FOR CONCRETE | 2008 |
|
RU2377205C1 |
METHOD OF PRODUCING OF DECORATIVE CONCRETE PRODUCTS | 2006 |
|
RU2330000C1 |
METHOD FOR MAKING CONCRETE ARTICLES HAVING PROTECTIVE-DECORATIVE COATING | 2006 |
|
RU2302335C1 |
METHOD FOR MANUFACTURING COARSE AGGREGATE FOR CONCRETE | 2007 |
|
RU2334712C1 |
CONCRETE MIXTURE | 2012 |
|
RU2500640C1 |
METHOD FOR MANUFACTURING OF COARSE FILLER FOR CONCRETES | 2008 |
|
RU2372304C1 |
METHOD FOR DECORATIVE CONCRETE ARTICLE PRODUCTION (VARIANTS) | 2006 |
|
RU2311291C1 |
METHOD FOR PRODUCTION OF DECORATIVE ARTICLE ON THE BASIS OF MINERAL BINDING AGENT | 2006 |
|
RU2320479C1 |
CONCRETE MIXTURE | 2012 |
|
RU2499778C1 |
Authors
Dates
2013-05-10—Published
2012-01-12—Filed