FIELD: chemistry.
SUBSTANCE: invention relates to composition of a concrete mixture and mortar and can be used in construction when making prefrabricated concrete or reinforced concrete articles and structures. The concrete mixture contains the following, wt %: portland cement 30.83-33.94; finely ground quartz sand with silicon dioxide SiO2 content higher than 94%, in which content of fine particles with average diameter smaller than 3.9 mcm is higher than 50% 1.78-3.55, river sand with fineness modulus of 1.9 55.5-56.00, Petrolafs additive 0.28-0.42, water - the balance.
EFFECT: high strength of concrete aged 12-24 hours, high bending and compression strength of concrete aged 28 days.
1 ex, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
FINE-GRAINED CONCRETE MIXTURE | 2017 |
|
RU2649996C1 |
HIGH STRENGTH SELF-COMPACTING FINE GRAIN CONCRETE | 2022 |
|
RU2796782C1 |
CONCRETE MIXTURE | 2012 |
|
RU2514060C2 |
COMPLEX ADDITIVE | 2007 |
|
RU2360879C1 |
METHOD OF THERMAL TREATMENT FOR CONCRETE AND REINFORCED CONCRETE ARTICLES | 2012 |
|
RU2519080C2 |
FINE-GRAINED CONCRETE AND METHOD OF THE CONCRETE MIXTURE PREPARATION FOR ITS PRODUCTION | 2017 |
|
RU2657303C1 |
COMPLEX ADDITIVE | 2014 |
|
RU2552565C1 |
DRY MORTAR | 2018 |
|
RU2681321C1 |
FINE-GRAINED SELF-COMPACTING CONCRETE MIX | 2022 |
|
RU2778123C1 |
HYBRID CEMENT | 2019 |
|
RU2716661C1 |
Authors
Dates
2013-05-20—Published
2011-11-30—Filed