FIELD: metallurgy.
SUBSTANCE: proposed method comprises smelting initial material to produce vitreous arsenic trisulfide. Arsenic-bearing sulfide cake is subjected to neutralisation given its moisture content does not exceed 0.5%. Smelting is performed in protective capsule preformed from liquid dump slag at 350-400°C using the heat of said dump slag. Then, buffer layer of heat-insulation material is formed on the surface of obtained cake melt. Now, said protective capsule is sealed by coating its surface with buffer layer of liquid dump slag to be hardened thereafter. Aforesaid heat-insulation layer represents crushed slag and/or quartz sand and/or undersized crushed stone.
EFFECT: higher efficiency.
2 cl, 1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR OBTAINING A NON-STOICHIOMETRIC ARSENIC POLYSULFIDE COMPOUND INSOLUBLE IN GROUNDWATER | 2021 |
|
RU2789975C1 |
METHOD OF DECONTAMINATING AND RECYCLING SULPHIDE ARSENIC-CONTAINING WASTES | 2019 |
|
RU2711766C1 |
METHOD FOR PRODUCTION OF WATER-INSOLUBLE WASTE OF ARSENIC SULFIDES | 2020 |
|
RU2747153C1 |
METHOD FOR PROCESSING ARSENIC-CONTAINING DUST OF NON-FERROUS METALLURGY | 2022 |
|
RU2785796C1 |
METHOD FOR COMPLEX PROCESSING OF POLYMETALLIC RAW MATERIALS | 1998 |
|
RU2181781C2 |
METHOD FOR PROCESSING INTERMEDIATE PRODUCTS OF LEAD PRODUCTION | 0 |
|
SU1122720A1 |
METHOD OF PROCESSING SULFIDE COPPER-NICKEL ORES AND CONCENTRATES | 0 |
|
SU1155624A1 |
METHOD OF BRINGING OUT ARSENIC FROM TECHNOLOGICAL PROCESS | 0 |
|
SU1497250A1 |
METHOD OF PRODUCTION OF BLISTER COPPER AND ZINC | 2004 |
|
RU2261285C1 |
METHOD OF TREATMENT HARD GOLD-ARSENICAL ORES AND CONCENTRATES AND FURNACE FOR ITS IMPLEMENTATION | 2007 |
|
RU2348713C1 |
Authors
Dates
2013-05-27—Published
2012-03-02—Filed