FIELD: construction.
SUBSTANCE: glazing contains the following components, wt %: scraps of window and/or container glass 49-50; kaolin 1-3; calcinated soda 12-15; phosphogypsum 13-15; borax 20-22. The prepared glazing charge is melted at 1000°C. The produced frit is ground, mixed, and a suspension is prepared, which is applied onto the surface of ceramic products. Baking is done at 850°C.
EFFECT: decreased temperature of glazing baking.