FIELD: construction.
SUBSTANCE: filler contains the following components, wt %: portland cement 33.0-36.0; water 25.6-28.0; bone glue 3.5-4.3; bone ash 32.5-37.7.
EFFECT: improving bond strength of a filler with concrete surface.
1 tbl