Abstract RU 2489407 C1

FIELD: construction.

SUBSTANCE: brick glaze contains the following components, wt %: clay 4-6; yellow lead 16-20; manganese peroxide 2-4; quartz sand 60-63; dry galvanic sludge 12-16. Temperature of glaze baking is 1050-1100°C. Frost resistance of the produced glaze makes 45-50 cycles.

EFFECT: increase of glaze frost resistance.

1 tbl

Similar patents RU2489407C1

Title Year Author Number
BRICK GLAZE 2012
  • Shchepochkina Julija Alekseevna
RU2489408C1
BRICK GLAZE 2012
  • Shchepochkina Julija Alekseevna
RU2508279C1
BRICK GLAZE 2012
  • Shchepochkina Julija Alekseevna
RU2507184C1
LUSTRELESS BLACK TILE GLAZE 2013
  • Shchepochkina Julija Alekseevna
RU2513493C1
BRICK GLAZE 2012
  • Shchepochkina Julija Alekseevna
RU2498966C1
GLAZE COMPOSITION 2012
  • Shchepochkina Julija Alekseevna
RU2481279C1
BRICK GLAZE 2012
  • Shchepochkina Julija Alekseevna
RU2496726C1
BRICK GLAZE 2012
  • Shchepochkina Julija Alekseevna
RU2489410C1
CRUDE MIXTURE FOR MAKING SILICATE BRICKS WITH PLASMA-MOLTEN BRICK FACE 2011
  • Shchepochkina Julija Alekseevna
RU2449964C1
GLAZE 2011
  • Shchepochkina Julija Alekseevna
RU2479556C1

RU 2 489 407 C1

Authors

Shchepochkina Julija Alekseevna

Dates

2013-08-10Published

2012-04-06Filed