FIELD: construction.
SUBSTANCE: method includes mixing of bitumen and rubber crumb of tyre wastes, their temperature treatment and mixture plasticising. Bitumen and rubber crumb in the composition are used at the following ratio, wt %: rubber crumb - 13.0-31.0, bitumen - balance. At the same time rubber crumb is added into bitumen pre-heated up to 160°C in portions with mixing, besides, after loading of its last portion the mixture is mixed for around 10 minutes. Then, while the mixture is being mixed, it is treated with ultrasound, upon completion of which the mixture is mixed for around 10 minutes.
EFFECT: rubber and bitumen compositions have higher values of softening and brittleness temperatures preserved in severe climatic conditions under higher mechanical loads.
5 cl, 1 tbl, 8 ex
Title | Year | Author | Number |
---|---|---|---|
PRODUCTION OF RUBBER-BITUMEN COMPOUND | 2012 |
|
RU2550888C2 |
METHOD TO PREPARE RUBBER MODIFIED BITUMEN | 2010 |
|
RU2448134C1 |
RUBBER-BITUMEN MASTIC | 2006 |
|
RU2323231C1 |
ELASTOMERIC OIL BITUMEN MODIFIER AND ELASTOMER-BITUMEN BINDER BASED THEREON | 2019 |
|
RU2701026C1 |
MODIFIED BITUMEN FOR CONSTRUCTION AND METHOD FOR ITS OBTAINING | 2023 |
|
RU2812072C1 |
LOW-TEMPERATURE METHOD OF PRODUCING MODIFIED RUBBER CRUMBS | 2020 |
|
RU2730857C1 |
BITUMEN-CONCRETE MIXTURE ON NANO-MODIFIED BINDER | 2013 |
|
RU2521988C1 |
RUBBER-CONTAINING POLYMERIC BITUMEN MODIFIER | 2004 |
|
RU2266934C1 |
COMPOSITE RUBBER-BITUMINOUS BINDER AND METHOD OF ITS OBTAINING | 2016 |
|
RU2655334C2 |
BITUMEN-RUBBER COMPOSITION AND METHOD FOR ITS PREPARING | 2002 |
|
RU2223990C2 |
Authors
Dates
2013-08-10—Published
2012-06-29—Filed