FIELD: weapons and ammunition.
SUBSTANCE: proposed method comprises two-step removal of moisture brought about by wetting from powder elements. First, moisture is displaced from powder elements by ethyl alcohol in concentration of 95-96% under centrifugal force in sprinkling of powder with alcohol in amount of 0.35-0.50 l/kg for fine powders and 0.50-1.00 l/kg for medium powders with simultaneous powder expression for 2-3 min and final expression for at least 10 min. Removal of residual amount of water-alcohol mix from powder to required magnitudes is performed by drying in table drier or dry-cure cabinets by air heated to 25-40°C for at least 1 hour with simultaneous forced discharge of used air or drying in 70 mmHg-vacuum for at least 1.5 h. Batch centrifuges are used for displacement.
EFFECT: fast and safe process, higher efficiency.
3 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR REMOVING HIGHLY VOLATILE SOLVENT FROM PYROXYLINE POWDER | 2014 |
|
RU2553291C1 |
METHOD OF PRODUCTION OF THE FINE-GRAIN COMBINED POWDERS | 2004 |
|
RU2285685C2 |
METHOD OF PREPARING POROUS PYROXYLIN POWDER FOR CARTRIDGES OF SMALL ARMS | 1996 |
|
RU2156230C2 |
POROUS PYROXYLIN POWDER FOR PROPELLANT CHARGES TO CARTRIDGES OF SMALL ARMS OF CIVIL PURPOSE | 2023 |
|
RU2820891C1 |
FUSIBLE COMPOSITION FOR EMULSIVE MODERATION OF POWDERS | 2010 |
|
RU2448073C2 |
MODULAR THROWING CHARGE (VERSIONS) AND METHOD OF ITS FABRICATION | 2012 |
|
RU2528984C2 |
DIBASIC PYROXYLIN POWDER PREPARATION METHOD | 2002 |
|
RU2242449C2 |
METHOD OF MANUFACTURING OF POROUS GUNCOTTON GUNPOWDER | 2006 |
|
RU2340585C2 |
METHOD FOR PRODUCTION OF POROUS PYROXYLIN GUN POWDER FOR CARTRIDGES FOR SHOOTING WEAPON | 1999 |
|
RU2165402C2 |
METHOD FOR PRODUCTION OF BIBASIC POWDER (VERSIONS) | 2007 |
|
RU2382020C2 |
Authors
Dates
2013-11-20—Published
2012-04-10—Filed