FIELD: construction.
SUBSTANCE: ceramic mass contains the following components, wt %: loess-like loam 89.8-90.8; kaolin 2.0-3.0; zinc oxide 0.2-0.3; fly ash 6.0-8.0.
EFFECT: increased frost resistance of items.
1 tbl