FIELD: metallurgy.
SUBSTANCE: alloy contains the following, wt %: up to 20 of sum of Co and Fe, between 17 and 21 Cr, between 0.5 and 3 of sum of Mo and W, not more than 2 Mo, between 4.8 and 6 Al, between 1.5 and 5 Ta, between 0.01 and 0.2 of sum of C and B, between 0.01 and 0.2 Zr, between 0.05 and 1.5 Hf, between 0.05 and 1.0 Si, and between 0.01 and 0.5 of sum of at least two elements of actinides and rare-earth metals, such as Sc, Y and lanthanides. Content of each element is not more than 0.3. Alloy is used in high-temperature components representing rotating blades, guide vanes, heat shields, seals or parts of a combustion chamber in gas turbines, as well as process alloy for repair welding and/or cladding of such high-temperature components.
EFFECT: alloy has high properties of stability to oxidation, resistance to high-temperature corrosion, strength and ductility, weldability.
21 cl
Title | Year | Author | Number |
---|---|---|---|
NICKEL-BASED SUPERALLOY WITH STRENGTHENING GAMMA-LINE-PHASE | 2009 |
|
RU2450067C1 |
NICKEL-BASED SUPER ALLOY HARDENED BY GAMMA-DASH PHASE | 2009 |
|
RU2441088C1 |
MONO-CRYSTAL SUPER-ALLOY ON BASE OF Ni AND TURBINE BLADE CONTAINING IT | 2008 |
|
RU2415959C1 |
SINGLE-CRYSTALLINE SUPERALLOY BASED ON Ni AND TURBINE BLADE COMPRISING IT | 2010 |
|
RU2482205C1 |
MONO-CRYSTAL SUPER-ALLOY ON BASE OF Ni | 2007 |
|
RU2415190C2 |
NICKEL-BASED SUPERALLOY | 2011 |
|
RU2567759C2 |
MONOCRYSTALLINE Ni-BASED SUPERALLOY AND TURBINE BLADE | 2010 |
|
RU2518838C2 |
METAL COATING WITH BINDER THAT FEATURES HIGH TEMPERATURE OF GAMMA/GAMMA' TRANSITION AND THE PART | 2010 |
|
RU2523185C2 |
HIGH-STRENGTH NICKEL-BASED SUPERALLOY RESISTANT TO HIGH-TEMPERATURE CORROSION AND OXIDATION, AND DIRECTIONALLY SOLIDIFIED PRODUCT OF THIS SUPERALLOY | 2002 |
|
RU2295585C2 |
NICKEL-BASED SUPERALLOY, MONOCRYSTALLINE BLADE AND TURBOMACHINE | 2018 |
|
RU2780326C2 |
Authors
Dates
2013-12-10—Published
2010-04-07—Filed