SUBSTANCE: mixture for making glaze contains wt %: kaolin 3.0-5.0; feldspar 12.0-16.0; quartz sand 57.0-58.0; chalk 1.0-2.0; tin oxide 5.0-7.0; zinc oxide 1.0-2.0; barium carbonate 1.0-2.0; cobalt sulphate 1.0-2.0; bone ash 12.0-16.0. The glaze has thermal stability of (heating at 100°C in boiling water - cooling to 15°C in water) 20 cycles. Parts of mixture for making glare are melted of temperature 1430 - 1450°C.
EFFECT: high thermal stability of the glaze.