FIELD: oil and gas industry.
SUBSTANCE: method for production of formed coke of carbon-containing material includes stages of oil semi-coke heating, pressure moulding with obtainment of green mouldings and their further cocking. Oil semi-coke is heated up to 350-400°C, at that oil semi-coke with carbon-to-hydrogen atomic ratio within range of (1.3-1.7) or oil semi-coke with carbon-to-hydrogen atomic ratio more than 1.7 is used with addition of sintering additives. After the heating stage before moulding the heated oil semi-coke is hold within 10-20 s.
EFFECT: invention allows improving quality of mouldings, simplifying the method and increasing technology stability and reliability, reducing energy costs and expanding sources of raw materials.
3 cl, 2 dwg, 1 tbl, 4 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR FORMING FINE FACTIONS OF OIL COKE | 2017 |
|
RU2660129C1 |
COMPOSITION OF CHARGE FOR PRODUCING METALLURGICAL COKE | 2020 |
|
RU2769188C1 |
METHOD OF MOULDED COKE PREPARING | 0 |
|
SU1798364A1 |
METHOD OF PREPARATION OF COAL CHARGE TO COKING | 1993 |
|
RU2039787C1 |
ADDITIVE TO CHARGES FOR MANUFACTURING METALLURGICAL COKE | 2017 |
|
RU2636514C1 |
0 |
|
SU218808A1 | |
0 |
|
SU356289A1 | |
OIL COKING ADDITIVE | 2016 |
|
RU2637965C1 |
METHOD OF THERMAL COAL ENRICHMENT | 2015 |
|
RU2637551C2 |
METHOD OF PREPARING COAL CHARGE FOR COKING | 0 |
|
SU1736994A1 |
Authors
Dates
2014-05-20—Published
2012-09-26—Filed