FIELD: machine building.
SUBSTANCE: heating for soldering is carried out in ring inductor at 1100-1150°C. Cutter hear is first cooled at the rate of 100-150°C/min in industrial oil "И-20A" at 60-80°C for 10-15 s. Then, the holder is placed in oil at 18-20°C and tempered at 200°C.
EFFECT: higher hardness.
3 tbl, 2 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MAKING HARD ALLOY CERMET ARTICLES | 1998 |
|
RU2145916C1 |
METHOD OF MANUFACTURING TOOL | 0 |
|
SU1139759A1 |
METHOD OF MAKING TOOL WITH SOLDERED HIGH-SPEED STEEL PLATES | 0 |
|
SU734302A1 |
METHOD FOR PRODUCING CUTTING TOOL WITH SOLDERED CUTTING TIP | 2005 |
|
RU2279338C1 |
CUTTING INSTRUMENT | 2006 |
|
RU2317875C1 |
METHOD FOR THERMAL TREATMENT OF CUTTING TOOLS FROM CARBIDE-CONTAINING HARD ALLOYS | 2020 |
|
RU2733081C1 |
HARD ALLOY TOOLS PRODUCTION METHOD | 1992 |
|
RU2043870C1 |
METHOD OF MANUFACTURING SOLDERED TOOLS | 0 |
|
SU1555380A1 |
METHOD OF WEAR-RESISTANT INDEXABLE PICK MANUFACTURE | 2016 |
|
RU2626481C1 |
METHOD OF THE CONTACT-REACTIVE SOLDERING OF STEEL | 1992 |
|
RU2042481C1 |
Authors
Dates
2014-05-27—Published
2013-04-09—Filed