FIELD: oil and gas industry.
SUBSTANCE: method can be applied in preparation of compounds mainly used for fixation of waterproof compounds in a horizontal well bore, for temporary formation blocking and setting of a supporting plug for offshoot kick-off. The method of compound preparation for production of acid-soluble plugging stone involves mixing microcalcite with 160-315 mcm particle size with plain oil-well portland cement, adding air-entraining agent "Aeroplast" to fresh water and mixing of plain oil-well portland cement with microcalcite using fresh water, with adding air-entraining agent "Aeroplast", with the following mixture ratio: plain oil-well portland cement - 59.9-64.95 weight fraction; microcalcite - 35-40 weight fraction; air-entraining agent "Aeroplast" - 0.05-0,1 weight fraction; fresh water - 50 weight fraction.
EFFECT: increased strength of acid-soluble plugging stone.
1 ex, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
ACID-SOLUBLE LIGHTWEIGHT PLUGGING MATERIAL TO LIQUIDATE ABSORPTION IN PRODUCTIVE FORMATIONS | 2014 |
|
RU2575489C1 |
METHOD FOR ELIMINATING BEHIND-CASING FLOWS AND INTER-CASING PRESSURE IN OIL AND GAS WELLS | 2014 |
|
RU2550116C1 |
EXPANDING PLUGGING MATERIAL WITH ADJUSTABLE DENSITY OF MORTAR | 2006 |
|
RU2401292C2 |
EXPANSION PLUGGING MATERIAL | 2007 |
|
RU2380392C2 |
POROUS EXPANDING CEMENT MATERIAL | 2023 |
|
RU2813584C1 |
WEIGHTED MINERALIZED GROUTING PORTLAND CEMENT COMPOSITION | 2022 |
|
RU2782526C1 |
GROUTING MORTAR | 2004 |
|
RU2261322C1 |
CEMENTING COMPOSITION | 2005 |
|
RU2302444C2 |
ACID-SOLUBLE BACKFILL COMPOSITION | 2010 |
|
RU2452757C1 |
PROCEDURE FOR WELL CEMENTING | 2007 |
|
RU2369722C2 |
Authors
Dates
2014-06-10—Published
2013-03-12—Filed