FIELD: chemistry.
SUBSTANCE: method of obtaining zirconium nitride consists in carrying out self-propagating high-temperature synthesis of an exothermic mixture, which consists of zirconium oxide and an energy component, in the presence of a nitriding agent. Heat-treatment of intermediate products is performed by interrupting the process of burning in 20-90 seconds after initiation; an activating additive of yttrium oxide nanopowder is additionally introduced into the exothermic mixture; zirconium nanopowder is used as the energy component. The size of zirconium oxide particles is 500-1000 times smaller than the size of zirconium particles, with the following component ratio, wt %: energy component - 60-100, zirconium oxide - 0-40, activating additive (introduced over 100%) - 1-3.
EFFECT: increased output of zirconium nitride with simplicity of its obtaining.
1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF METAL NITRIDES PREPARATION | 2007 |
|
RU2355631C1 |
METHOD FOR PREPARING METAL NITRIDES | 2003 |
|
RU2256604C2 |
METHOD OF PRODUCING ALUMINIUM NITRIDE | 2010 |
|
RU2428376C1 |
METHOD OF PRODUCING POWDER COMPOSITIONS BASED ON NITRIDES OF ELEMENTS | 1998 |
|
RU2163181C2 |
METHOD OF PREPARING OF SIALONE POWDER | 1990 |
|
RU1774612C |
β′ SIALON POWDER PRODUCTION METHOD | 1989 |
|
SU1626601A1 |
METHOD OF PRODUCING COMPOSITE CERAMIC MATERIAL | 2013 |
|
RU2524061C1 |
METHOD OF PRODUCING SILICON NITRIDE-BASED SINTERED ARTICLES | 2011 |
|
RU2458023C1 |
METHOD OF CONTROLLING RATE OF COMBUSTION OF MIXED SOLID FUEL | 2008 |
|
RU2423338C2 |
THERMITE FUEL COMPOSITION | 2010 |
|
RU2418779C1 |
Authors
Dates
2014-07-20—Published
2012-12-11—Filed