FIELD: chemistry.
SUBSTANCE: solution contains, g/l: nickel dichloride 10-15, succinic acid 12-15, sodium fluoride 2-3, sodium hydroxide 4-6, sodium hypophosphite 17-20, copper-polymer complex of polyvinyl pyrrolidone 2.0-6.0, potassium polytitanate 10-30, distilled water - the balance.
EFFECT: solution enables to obtain composite coatings, having high wear resistance and low coefficient of friction, which prolongs the service life of friction assemblies.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
SOLUTION FOR CHEMICAL PRECIPITATION OF COMPOSITE NICKEL-PHOSPHORUS COATINGS | 2013 |
|
RU2531219C1 |
SOLUTION FOR CHEMICAL DEPOSITION OF NICKEL COATINGS | 2013 |
|
RU2516188C1 |
SOLUTION FOR CHEMICAL DEPOSITION OF NICKEL-PHOSPHORIC COATINGS | 2007 |
|
RU2354746C2 |
SOLUTION FOR PREPARING COMPOSITION COVER WITH CHEMICAL PRECIPITATION | 2005 |
|
RU2287612C1 |
SOLUTION FOR CHEMICAL PRECIPITATION OF COMPOSITE NICKEL COVERS | 2003 |
|
RU2235803C1 |
SOLUTION FOR CHEMICALLY DEPOSITING PROTECTIVE COATING ON POWDER STEELS | 2005 |
|
RU2298594C1 |
METHOD FOR OBTAINING NICKEL COATING ON MATERIALS FROM CARBON FIBRES | 2006 |
|
RU2334020C1 |
SOLUTION TO PRODUCE COMPOSITE COATING | 2012 |
|
RU2491370C1 |
SOLUTION FOR CHEMICAL DEPOSITION OF COMPOSITION NICKEL COATINGS | 1995 |
|
RU2108416C1 |
APPLICATION OF BIS(4-R-2-AMINOPHENYL) DISULFIDE AS A LEVELING AGENT IN A SOLUTION FOR THE CHEMICAL DEPOSITION OF NICKEL-PHOSPHORUS COATINGS | 2023 |
|
RU2813159C1 |
Authors
Dates
2014-07-27—Published
2013-05-08—Filed