FIELD: metallurgy.
SUBSTANCE: invention relates to nonferrous metallurgy. Copper-electrolyte sludge is dressed. Compounds of lead and stibium are removed from dressed sludge to be mixed with cathode product of leaching of selenium from copper-electrolyte sludge at 5-10:1 ratio. Then, cathode leaching in alkaline electrolyte from obtained mix is performed at current density of 2000-3000 A/m2. To prevent selenium circulation between cathode and anode, the latter are separated by web permeable for electrolyte.
EFFECT: two - two and a half-fold increase in selenium cathode leaching, one and a half - two-fold decrease in selenium content in sludge.
1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
PROCESSING METHOD OF COPPER ANODE SLIME | 2015 |
|
RU2618050C1 |
METHOD OF EXTRACTING ANTIMONY AND LEAD | 2015 |
|
RU2590781C1 |
PROCESS CONDITIONING LEAD-CARRYING MATERIAL BEFORE SMELTING | 1998 |
|
RU2131473C1 |
METHOD OF PROCESSING COPPER-ELECTROLYTE SLUDGES | 1997 |
|
RU2109823C1 |
PROCEDURE FOR TREATMENT OF ZINC CONTAINING GOLD-SILVER AND/OR SILVER-GOLD CAKES WITH EXTRACTION OF VALUABLE COMPONENTS | 2010 |
|
RU2424338C1 |
METHOD OF COPPER-ELECTROLYTE SLIME PROCESSING | 1992 |
|
RU2071978C1 |
METHOD OF PRODUCING OF HIGH PURITY COPPER | 2017 |
|
RU2667927C1 |
METHOD OF OBTAINING ANTIMONY FROM CONCENTRATE | 2002 |
|
RU2219267C1 |
PROCESSING METHOD OF COPPER ANODE SLIME | 2013 |
|
RU2550064C2 |
METHOD OF COPPER ELECTROREFINING LEADED SLIMES TREATMENT (VERSIONS) | 2011 |
|
RU2451759C1 |
Authors
Dates
2014-11-27—Published
2013-03-12—Filed