FIELD: chemistry.
SUBSTANCE: method involves the addition of an aqueous emulsion, comprising a reactive sizing agent and an insolubilising agent, either separately or in a blended form to aqueous pulp slurry and forming the slurry into cardboard or paperboard. The reactive sizing agent comprises at least 30 wt % of a linear saturated fatty acid anhydride C14-22. The insolubilising agent selected from the group consisting of alum (aluminium sulphate) and polyaluminumchloride (PAC).
EFFECT: invention makes it possible to increase the paperboard resistance to hot hydrogen peroxide solution and lactic acid.
10 cl, 9 tbl, 6 ex
Title | Year | Author | Number |
---|---|---|---|
GLUING COMPOSITIONS | 2012 |
|
RU2602061C2 |
METHOD OF MANUFACTURING FLUIDS-PACKAGING COATED CARDBOARD | 1998 |
|
RU2190717C1 |
SIZING COMPOSITION | 2000 |
|
RU2211274C2 |
PAPER IMPREGNATION | 1998 |
|
RU2169224C2 |
GLUE COMPOSITION FOR PAPER | 2010 |
|
RU2564817C2 |
OIL AND WATER EMULSIFICATION APPARATUS, SYSTEM AND PROCESS | 2009 |
|
RU2538578C2 |
PACKING LAMINATE | 2007 |
|
RU2455169C2 |
PROCESS FOR MANUFACTURING FLUID FOOD PRODUCTS PACKING BOARD | 0 |
|
SU1807147A1 |
METHOD OF FABRICATING GLUED PAPER, PAPERBOARD, BOARD, AND SIMILAR PRODUCTS FROM CELLULOSE FIBERS, AND AQUEOUS DISPERSION OF GLUING AGENTS | 1995 |
|
RU2097464C1 |
METHOD FOR MANUFACTURING OF CARDBOARD AND METHOD FOR REDUCING MOISTURE-PERMEABILITY OF CARDBOARD | 2002 |
|
RU2303673C2 |
Authors
Dates
2015-05-27—Published
2010-07-22—Filed