FIELD: metallurgy.
SUBSTANCE: invention relates to metallurgy and can be used at the production of ferromolybdenum with copper content of 0.5% from low-grade molybdenite with high copper content. According to the method, the following is performed: addition of iron and metallic aluminium to molybdenite with copper content of 0.5-10% and their mixing, reaction of the mixture in the heater at a temperature of 1100-2000°C in a gaseous argon atmosphere and natural cooling of the molten metal at an ambient temperature after the reaction is finished so that ferromolybdenum with copper content of less than 0.5 wt % is obtained.
EFFECT: invention allows reducing the consumption of a reducing agent - aluminium - due to direct reduction without any oxidation process by using molybdenite with high copper content.
6 cl, 2 dwg, 2 tbl, 6 ex
Title | Year | Author | Number |
---|---|---|---|
CHARGE AND METHOD FOR ALUMINOTHERMIC PRODUCTION OF FERROMOLYBDENUM USING IT | 2012 |
|
RU2506338C1 |
METHOD FOR PRODUCING FERROMOLYBDENUM | 1994 |
|
RU2110596C1 |
CHARGE FOR OBTAINING FERROMOLYBDENUM IN BURNING MODE | 1990 |
|
RU2044791C1 |
SINTERED AGGLOMERATES AND METHOD FOR PRODUCING THE SAME | 2000 |
|
RU2244025C2 |
METHOD OF PRODUCTION OF AGENT SELECTED FROM SERIES: BORON, PHOSPHORUS, SILICON AND RARE-EARTH METALS (VERSIONS) | 2005 |
|
RU2298589C2 |
METALLOTHERMIC PROCESS FOR EXTRACTING RARE-EARTH METALS FROM THEIR FLUORIDES FOR PRODUCING ALLOYS AND CHARGE FOR PERFORMING SUCH PROCESS | 2001 |
|
RU2181784C1 |
PROCEDURE FOR TREATMENT OF MOLYBDENUM CONCENTRATE (VERSIONS) | 2008 |
|
RU2434066C2 |
METHOD OF CHARGE PREPARATION FOR FERROMOLYBDENUM PRODUCTION | 1994 |
|
RU2078843C1 |
EXOTHERMIC MIXTURE FOR ALLOYING OF IRON-CARBON ALLOYS WITH MOLYBDENUM | 1995 |
|
RU2098489C1 |
METHOD FOR PRODUCTION OF SYNTHETIC SLAG AND ALLOY FOR ALLOYING STEELS WITH NICKEL AND MOLYBDENUM | 1989 |
|
SU1678055A1 |
Authors
Dates
2015-06-10—Published
2010-10-20—Filed