FIELD: metallurgy.
SUBSTANCE: steel microalloying by boron is performed at output by the addition to the ladle of the aluminium and complex alloy of ferrosilicon boron in amount of 4.0-7.5 kg/t of steel with ratio of aluminium to ferrosilicon boron within range (0.25-0.50), at that the ferrosilicon boron contains in wt %: 60-65 Si and 0.5-2.0 B.
EFFECT: reduced expenses for metal production, reduced time of out of furnace treatment at ladle-furnace unit, and increased quality of the metal products.
2 cl, 1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD OF MICROALLOYING OF STEEL BY BORON | 1991 |
|
RU2016087C1 |
| METHOD OF STEEL PRODUCTION | 2006 |
|
RU2334796C1 |
| MANUFACTURING METHOD OF BORON STEEL | 2008 |
|
RU2382086C1 |
| METHOD OF DEOXIDATION, MICROALLOYING AND MODIFYING OF RAIL STEEL | 1991 |
|
RU2033433C1 |
| FIREPROOF STEEL PRODUCTION METHOD | 2023 |
|
RU2807799C1 |
| BORON STEEL MAKING METHOD | 2011 |
|
RU2477324C1 |
| COMPLEX ALLOY FOR MICROALLOYING AND DEOXIDATION OF IRON-BASED STEEL | 2019 |
|
RU2715510C1 |
| METHOD FOR PRODUCTION OF ELECTRO-WELDED PIPE MADE OF LOW-CARBON STEEL, RESISTANT TO HYDROGEN CRACKING (OPTIONS) | 2020 |
|
RU2747083C1 |
| METHOD OF PRODUCING BORON-CONTAINING STEEL | 2011 |
|
RU2492248C2 |
| STEEL INGOT PRODUCTION METHOD | 0 |
|
SU996070A1 |
Authors
Dates
2015-09-20—Published
2014-07-03—Filed