FIELD: chemistry.
SUBSTANCE: invention relates to caoutchouc composition and tyre. Caoutchouc composition is obtained by mixing and batching caoutchouc component with hydrated silicon dioxide. Average diameter of primary particle D and logarithm of differential volume of pores LP in silicon dioxide with pore diameter of hydrated silicon dioxide, extracted from mixed and batched caoutchouc composition, 30 nm satisfy ratios, presented by formulae LP> - 0.045 x D + 1.45 (1) and D < 30 nm (2) at any value D, satisfying formula (2).
EFFECT: invention makes it possible to obtain good wear resistance without deterioration of tyre rolling resistance.
6 cl, 4 dwg, 6 tbl, 8 ex
Title | Year | Author | Number |
---|---|---|---|
RUBBER MIXTURE AND ITS APPLICATION IN PNEUMATIC TYRE | 2011 |
|
RU2540629C2 |
TIRE MADE USING RUBBER COMPOSITION CONTAINING MODIFIED POLYMER | 2009 |
|
RU2475368C2 |
RUBBER COMPOSITION AND TIRE | 2012 |
|
RU2613969C2 |
METHOD FOR OBTAINING VULCANISED CAOUTCHOUC COMPOSITION | 2011 |
|
RU2575657C2 |
RUBBER COMPOSITION AND TYRE | 2013 |
|
RU2617481C2 |
RUBBER COMPOSITION AND TIRE | 2012 |
|
RU2611511C2 |
COPOLYMER, RUBBER COMPOSITION WITH ITS USE AND TIRE | 2013 |
|
RU2629197C2 |
COPOLYMER, RUBBER COMPOSITION WITH ITS USE, AND TIRE | 2013 |
|
RU2621032C2 |
COPOLYMER, RUBBER COMPOSITION WITH ITS USE AND TIRE | 2013 |
|
RU2631318C2 |
DIENE RUBBER AND RUBBER COMPOSITION | 2020 |
|
RU2799596C2 |
Authors
Dates
2016-01-27—Published
2012-08-31—Filed